Paper and cardboard thickness meter TP-E21

Paper and cardboard thickness meter TP-E21 measures thickness of paper, corrugated papers using contact measurement method. The Analogue (pointer type) type gauge display is mounted at top with a false weight so as to develop a uniform, reproducible constant pressure on the anvil through the foot. It finds applications in paper, printing, and packaging industry.

  • Sample size (L*B)
    Rub pressure
    Friction speed
    Friction area (L*B)
    No. of friction
    Measuring range 0 to 20 mm
    Division value
    Accuracy 0.01 mm
    Gauge Analogue gauge display
    Contact pressure (to create false weight) 20 ± 0.5 kPa
    Contact diameter 35.7 ± 0.5 mm
    Error of depth parallelism 0.03 mm
    Testing speed
    Test range
    Indicating Error ± 0.0025 mm or ± 0.5 %
    Indication variability ≤ 0.0025 mm or ≤ 0.5 %
    Pressing depth of the measuring head
    Parallelism error between two brims of the specimen stages
    Slit width of the specimen stage
    Testing length
    Sample size
    Bend angle
    Sample width
    Sample maximum length
    Parallelism
    Dimension 233×160×120 mm
    Weight 5.5 kg
    Power supply
    • Portable, compact design
    • Measuring range 0 to 20 mm for corrugated paper
    • Incorporated with contact measurement method
    • Analogue gauge display
    • Manual operations
    • Easy to use
  • Thickness tester is used to measure thickness of paper, corrugated paper, cardboard & other sheets widely used in paper testing, printing, packaging industry.

Automatic horizontal tensile tester TP-B11

  • 90 to 200 mmSample (size) length
  • 15 mm, 25 mm, 50mmSample width
  • 0 to 30, 0 to 100 N,0 to 300 NMeasuring range
  • ± 1 %Accuracy

Whiteness meter TP-A11

  • Diameter ≥30 mm, Thickness ≤ 40 mmSample (size) length
  • D/0 lighting geometrical viewing conditions, diffuser diameter (d) 150mm, testing hole diameter 30mmSystem
  • D65 as illuminating sourceLight source
  • ≤ 0.1 %Zero drift

Pulp beating (refining) freeness tester TP-C10

  • 0 to 100° SRMeasurement range
  • 100 ± 10 mm/sSealed testing speed
  • 1000 ± 5 mlVolume of distilled water
  • 149 ± 1 sDraining time
Internal Ply bond Tester TP-J11
  • A: 20 to 500 J/m2 B: 500 to 1000 J/m2Capacity
  • 90°Impact angle
  • Lb-ft/in2  J/m2Unit
  • A: ± 1 J/m2 B: ± 2 J/m2Error
Paper and cardboard thickness meter TP-E20
  • 0 to 4 mmMeasuring range
  • 0.01 or 0.001 mmAccuracy
  • Analogue gauge displayGauge
  • 100 ± 10 kPaContact pressure (to create false weight)

Vertical tensile tester TP-B20

  • 0 to 200 mm adjustableSample (size) length
  • 15 mmSample width
  • 0 to 30 N (tissue paper), 0 to 100 N,0 to 300 N, 0 to 500 N, 0 to 1000 NMeasuring range
  • ± 1 %Accuracy

Crush tester TP-L10

  • 5 to 500 N, 50 to 3000 NMeasurement range
  • 1 NResolution
  • ± 1 %Accuracy
  • ≤ 1 %Variability

Electronic Tearing tester TP-J21

  • 10 -16000 mNCapacity
  • 0.1 mNResolution
  • 104 ± 1 mmTearing arm
  • 27.5° ± 5°Tearing angle
Coefficient of friction tester TP-D10
  • 0.01 to 10 NMeasurement range
  • 200 gSlider weight
  • 63×63 mmSlider size
  • ± 2 %Testing accuracy
Paper tearing tester TP-J20
  • 0 to 1000 mNMeasuring range
  • 0.1 mNResolution
  • ± 1 %Indication error
  • 104 ± 1 mmTearing arm

Whiteness and chromaticity tester TP-A10

  • Diameter ≥30 mm, Thickness ≤ 40 mmSample (size) length
  • Diffuse reflection factor Rx, Ry, Rz, stimulus value Y10, X10, Z10, chromaticity coordinates x10, y10, z10; lightness L *, chroma a * b *, chroma C * ab, hue angle h * ab, dominant wavelength λd, excitement purity Pe, color difference ΔE * ab, lightness difference ΔL *, chroma difference ΔC * ab, hue difference ΔH * ab, Hunter system L , A, bMeasurement mode
  • ≤ 0.1 within 30 minStability
  • Chromaticity co-ordinate 0.0001Accuracy

Ink rubber tester TP-F10

  • 230×50 mm (can join short samples together)Sample size (L*B)
  • 20 ± 0.2 NRub pressure
  • 43 times / minFriction speed
  • 155×50 mmFriction area (L*B)

Standard strip cutter TP-G10

  • 15 mmSample width
  • 300 mmSample maximum length
  • ≤ 0.1 mmParallelism
  • 240×520×70 mmDimension
Tensile Stiffness Tester TP-B10
  • 38×70 mmSample (size) length
  • (1-500) mN.m (divided into 7 small ranges)Measuring range
  • 0.02Indication error
  • (200° ± 20°)/ minTest speed
Mullen burst tester TP-K10
  • 0 to 5600 kPaMeasurement range
  • ± 0.5 % F.S.Accuracy
  • 170 ± 15 ml/minCompression speed
  • ≥ 690 kPaClamp pressure

Rockwell hardness meter TRHM-A11

  • 98 NPreliminary test force
  • 588, 980, 1471 NTotal test force
  • 1 to 30 STotal test force dwell time
  • Digital displayHardness indication

Rockwell hardness meter (motorized type) TRHM-B10

  • 98 NPreliminary test force
  • 588, 980, 1471 NTotal test force
  • 306, 613, 1839 NBrinell hardness test
  • 294, 588, 980 NVickers hardness test
Rockwell hardness meter TRHM-A10
  • 98 NPreliminary test force
  • 588, 980, 1471 NTotal test force
  • 0 to 30 STotal test force dwell time
  • Analogue displayHardness indication
Rubber Low Temperature Brittleness Tester TRBT-A11
  • Room temperature to -70 ℃ (room temperature ≤ 25 ℃)Temperature control range
  • ± 0.3 ℃Temperature accuracy
  • 0℃ to -30℃ around 2.5 ℃/min
    -30℃ to -40℃ around 2.5 ℃/min
    -40℃ to -70℃ around 2.0 ℃/min
    Impact speed
  • 910 × 510 × 860 mmMax dimension L × W × H

Three roll mill machine TRMM-A10

  • 0.5 to 1 kg, 2 to 3 kg, 5 to 7 kgMixed capacity
  • RT to 300°CTemperature range
  • PID controlTemperature control system
  • LED displayDisplay

DIN abrasion tester TDAT-A10

  • 2.5 NTest arm weight
  • 2.5 ± 0.1 N, 5 ± 0.1 N, 10 ± 0.1 N,Additional Loads
  • 150 mmIdler
  • 40 ± 0.2 MAbrasion stroke
Soil nutrient tester TSNA-A11
  • 0.001 to 9999Measuring range
  • A (absorbency of light) <0.003 within 3 minsStability
  • <3.0 %Linearity error
  • A (absorbency of light) <0.005Repeatability error
Soil Salinity tester TSST-A10
  • 0.00 to 19.99 ms/cmSalinity Measurement range
  • EC ± 2% full scaleMeasuring accuracy
  • -5 to 50°CTemperature Measurement range
  • ± 0.5°CTemperature accuracy

Soil nutrient tester TSNA-A10

  • 0.001 to 9999Measuring range
  • A (absorbency of light) <0.003 within 3 minsStability
  • <3.0 %Linearity error
  • A (absorbency of light) <0.005Repeatability error

Benchtop gloss meter TBGM-A10

  • 60°Test angle
  • 2 × 3 mmGloss aperture
  • 0 to 1000 GUMeasurement range
  • 0.2 GU (0 to 100 GU), 0.2 % GU (100 to 1000 GU)Repeatability
Whiteness meter TP-A11
  • Diameter ≥30 mm, Thickness ≤ 40 mmSample (size) length
  • D/0 lighting geometrical viewing conditions, diffuser diameter (d) 150mm, testing hole diameter 30mmSystem
  • D65 as illuminating sourceLight source
  • ≤ 0.1 %Zero drift
Whiteness and chromaticity tester TP-A10
  • Diameter ≥30 mm, Thickness ≤ 40 mmSample (size) length
  • Diffuse reflection factor Rx, Ry, Rz, stimulus value Y10, X10, Z10, chromaticity coordinates x10, y10, z10; lightness L *, chroma a * b *, chroma C * ab, hue angle h * ab, dominant wavelength λd, excitement purity Pe, color difference ΔE * ab, lightness difference ΔL *, chroma difference ΔC * ab, hue difference ΔH * ab, Hunter system L , A, bMeasurement mode
  • ≤ 0.1 within 30 minStability
  • Chromaticity co-ordinate 0.0001Accuracy

Tensile Stiffness Tester TP-B10

  • 38×70 mmSample (size) length
  • (1-500) mN.m (divided into 7 small ranges)Measuring range
  • 0.02Indication error
  • (200° ± 20°)/ minTest speed